Differential scanning calorimetry fingerprints of various heat-treatment tempers of different aluminum alloys
https://doi.org/10.3390/met10060763 “Heat-treatable cast and wrought aluminum alloys are widely used for structural applications in the automobile and aerospace industries. To assess and diagnose the production